We are providing wide range of whole tyre reclaim rubber and these are quality tested at our quality testing unit. With high quality standard and strict quality control system, these range meet the international standard.
Whole Tyre Reclaim Rubber (Superfine Grade)
|
|
|
SUPERFINE |
|
|
RTRR-11 |
Test Name |
Test Method |
Content |
Ash Content (%) |
ASTM D297-18 |
6 - 9 |
Carbon Black (%) |
ASTM E1131 |
18 - 27 |
Acetone Extract (%) |
ASTM D297-18 |
6 - 16 |
RHC (%) |
ASTM E1131 |
47 Min. |
|
Test Name |
Test Method |
Content |
Specific Gravity (gm/cc) |
ASTM D297-18 |
1.14 Max. |
Tensile Strength (kg/cm²) |
ASTM D412 |
40 Min. |
Elogation At Break (%) |
ASTM D412 |
200 Min. |
Mooney Viscosity (ml) |
ASTM D1646 |
35 - 55 |
Hardness (Shore A) |
ASTM 2240 |
55 - 65 |
|
Whole Tyre Reclaim Rubber (Fine Grade)
|
|
|
FINE |
|
|
RTRR-22 |
Test Name |
Test Method |
Content |
Ash Content (%) |
ASTM D297-18 |
6 – 9 |
Carbon Black (%) |
ASTM E1131 |
18 - 27 |
Acetone Extract (%) |
ASTM D297-18 |
6 - 16 |
RHC (%) |
ASTM E1131 |
47 Min. |
|
Test Name |
Test Method |
Content |
Specific Gravity (gm/cc) |
ASTM D297-18 |
1.14 Max. |
Tensile Strength (kg/cm²) |
ASTM D412 |
40 Min. |
Elogation At Break (%) |
ASTM D412 |
200 Min. |
Mooney Viscosity (ml) |
ASTM D1646 |
35 - 55 |
Hardness (Shore A) |
ASTM 2240 |
55 - 65 |
|
Whole Tyre Reclaim Rubber (Medium Grade)
|
|
|
MEDIUM |
|
|
RTRR-33 |
Test Name |
Test Method |
Content |
Ash Content (%) |
ASTM D297-18 |
6 - 9 |
Carbon Black (%) |
ASTM E1131 |
18 - 27 |
Acetone Extract (%) |
ASTM D297-18 |
6 - 16 |
RHC (%) |
ASTM E1131 |
47 Min. |
|
Test Name |
Test Method |
Content |
Specific Gravity (gm/cc) |
ASTM D297-18 |
1.14 Max. |
Tensile Strength (kg/cm²) |
ASTM D412 |
35 Min. |
Elogation At Break (%) |
ASTM D412 |
200 Min. |
Mooney Viscosity (ml) |
ASTM D1646 |
35 - 55 |
Hardness (Shore A) |
ASTM 2240 |
55 - 65 |
|
Whole Tyre Reclaim Rubber (High Tensile Grade)
|
|
|
High Tensile |
|
|
RTRR-55 |
Test Name |
Test Method |
Content |
Ash Content (%) |
ASTM D297-18 |
9 Max. |
Carbon Black (%) |
ASTM E1131 |
18 - 30 |
Acetone Extract (%) |
ASTM D297-18 |
6 - 16 |
RHC (%) |
ASTM E1131 |
48 Min. |
|
Test Name |
Test Method |
Content |
Specific Gravity (gm/cc) |
ASTM D297-18 |
1.14 Max. |
Tensile Strength (kg/cm²) |
ASTM D412 |
75 Min. |
Elogation At Break (%) |
ASTM D412 |
250 Min. |
Mooney Viscosity (ml) |
ASTM D1646 |
40 - 60 |
Hardness (Shore A) |
ASTM 2240 |
55 - 65 |
|
Application:
Reclaim rubber widely used in Truck Tyres, Tread Rubber and Rubber Moulded Components. Moderately refined reclaim rubber mainly used in Cycle Tyres, Rubber Mat, Battery Containers and also in molded rubber products. Coarse reclaim rubber mainly used in Tyre Flaps, Matts, Pedal Rubber, Rubber Sheets Floor/ Coir Matt etc...
Advantages:
- Shorter and faster mixing cycles.
- Improved die swell, adhesion, permeability.
- Reduction in consumption of electrical power due to nerve of compound and faster mixing cycle.
- Practically no reduction in hot air ageing properties.
- Fewer compounds at less cost.
- Low calendaring and extrusion temperature.